By BoDuan ·
Uneven Leather Skiving: Thickness Variation or a Wandering Skive Band?
When a skived edge looks uneven, check where the cut starts and how much leather remains. A strip can keep a straight boundary while its residual thickness changes. It can also wander sideways while the thickness inside the band stays consistent. Record both before changing the setup.

Compare the width of the band and measure the remaining thickness at three matching stations. The top view shows where to measure width; use a thickness gauge to check the remaining leather.
Compare the start, middle and end of a straight strip
Mark three stations across the back of a straight offcut and keep an uncut strip from the same piece. At each station measure from the original edge to the start of the bevel. Take a separate thickness reading at the same offset from the original edge, within the intended band. Keep the material relaxed and use the same gauge pressure across the readings, especially on soft leather.
If the band stays the same width while the remaining thickness changes, compare the marked positions with the original strip before asking the technician to check the cutting setup. If the boundary drifts, compare a straight control with the production part. Drift on the control warrants a check of the edge guide and how the strip seats against it. Drift only on a shaped part warrants a closer look at the feed path through its turns.
Record the result before changing another setting
Keep the two strips and photograph them grain side up and flesh side up. Write down which sample, setting and feed direction produced each result. The Fortuna ES 50 operating manual lists knife condition, presser-foot wear and worn stops among potential sources of poor skiving. Ask qualified personnel to follow the manual for the machine on the bench when inspecting or adjusting it.
View the BD-102 leather edge skiving machine if you are comparing machines. Ask for both measurements on straight and shaped pieces from your own material before choosing a configuration.
What to send for a skiving trial
Send one uncut strip and two strips that show the defect. Mark the feed direction, where the symptom starts, the desired band width and the target thickness at a specified distance from the edge. Include the finished overlap or fold if its fit is the reason for the trial.
Use the width and thickness measuring guide and the sample preparation checklist.
Discuss a BD-102 leather edge skiving trial →